Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact strength.Regulatory Status: NA967000 meets the requirements of the Food and Drug Administration, 21 CFR 177.1520. This regulation allows the use of this olefin polymer "...in articles or components of articles intended for use in contact with food," except in cooking applications. Specific limitations or conditions of use do apply. Contact your Equistar sales representative for more information. Specific recommendations for processing NA967000 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 1.5 g/10 min
1.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
molding; ASTM D2240
Tensile Strength at Break 10.3 MPa
1500 psi
molding; ASTM D638
Film Elongation at Break, MD 220 %
220 %
ASTM D882
Film Elongation at Break, TD 520 %
520 %
ASTM D882
Elongation at Break 600 %
600 %
molding; ASTM D638
Elmendorf Tear Strength MD 390 g
390 g
ASTM D1922
Elmendorf Tear Strength TD 100 g
100 g
ASTM D1922
Dart Drop 4.72 g/micron
120 g/mil
F<sub>50</sub>; ASTM D1709
Film Tensile Strength at Break, MD 24.8 MPa
3600 psi
ASTM D882
Film Tensile Strength at Break, TD 17.9 MPa
2600 psi
ASTM D882
1% Secant Modulus, MD 179 MPa
26000 psi
ASTM D882
1% Secant Modulus, TD 228 MPa
33000 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
molding; ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
molding; ASTM D746
0.500 °C
32.9 °F
molding, notched; ASTM D746
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F
Die Opening 0.0635 cm
0.0250 in
Blow-up Ratio (BUR) 2.0
2.0