MV Labs BI700 Bi(NO3)3·5H2O Bismuth nitrate pentahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF MV Labs BI700 Bi(NO3)3·5H2O Bismuth nitrate pentahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 458.07 g/mol
458.07 g/mol
Descriptive Properties Value Comments
Assay 43% Bi
CAS Number 10035-06-0
Form White crystals
Purity 99.999%
Typical Impurities Fe, Pb = 3 ppm; Ag, Cu = 1 ppm