| Category | Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® HTN |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.57 g/cc | 0.0567 lb/in³ | DAM; ISO 1183 |
| Water Absorption | 3.6 % <br>@Thickness 2.00 mm |
3.6 % <br>@Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 230 MPa | 33400 psi | 50%RH; ISO 527-1/-2 |
| 240 MPa | 34800 psi | DAM; ISO 527-1/-2 | |
| Elongation at Break | 2.0 % | 2.0 % | 50%RH; ISO 527-1/-2 |
| 2.3 % | 2.3 % | DAM; ISO 527-1/-2 | |
| Tensile Modulus | 15.0 GPa | 2180 ksi | DAM; ISO 527-1/-2 |
| 15.5 GPa | 2250 ksi | 50%RH; ISO 527-1/-2 | |
| Flexural Modulus | 13.2 GPa | 1910 ksi | DAM; ISO 178 |
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | DAM; ISO 180/1A |
| 13.0 kJ/m² <br>@Temperature -40.0 °C |
6.19 ft-lb/in² <br>@Temperature -40.0 °F |
DAM; ISO 180/1A | |
| Charpy Impact Unnotched | 8.50 J/cm² | 40.4 ft-lb/in² | DAM; ISO 179/1eU |
| 8.00 J/cm² <br>@Temperature -30.0 °C |
38.1 ft-lb/in² <br>@Temperature -22.0 °F |
DAM; ISO 179/1eU | |
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | DAM; ISO 179/1eA |
| 1.20 J/cm² <br>@Temperature -30.0 °C |
5.71 ft-lb/in² <br>@Temperature -22.0 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 300 °C | 572 °F | DAM; first heat; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 285 °C | 545 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | DAM; ISO 75-1/-2 |
| Flammability, UL94 | HB <br>@Thickness 1.50 mm |
HB <br>@Thickness 0.0591 in |
DAM; IEC 60695-11-10 |
| HB <br>@Thickness 0.800 mm |
HB <br>@Thickness 0.0315 in |
DAM; IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | DAM; IEC 60093 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Part Marking Code | >PA6T/XT-GF45< | ISO 11469 |
| >PPA-GF45< | SAE J1344 | |
| Processing | Injection Moulding | |
| Regional Availability | Asia Pacific | |
| Europe | ||
| Global | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Special Characteristics | Heat stabilised or stable to heat | |
| UL recognition | UL | DAM |