MV Labs RE850 NH4ReO4 Ammonium perrhenate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs RE850 NH4ReO4 Ammonium perrhenate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 268.24 g/mol
268.24 g/mol
Descriptive Properties Value Comments
Assay 69% Re
CAS Number 13598-65-7
Form White crystals
Purity 99.999%
Typical Impurities Fe, Mo, W = 3 ppm