Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
Tensile Strength, Ultimate 27.6 MPa
4000 psi
Machine direction
Flexural Yield Strength 48.3 MPa
7010 psi
Flexural Modulus 1.70 GPa
247 ksi
Izod Impact, Notched 4.30 J/cm
8.06 ft-lb/in
1.10 J/cm

@Temperature -29.0 °C
2.06 ft-lb/in

@Temperature -20.2 °F
Gardner Impact >= 32.0 J
>= 23.6 ft-lb
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F