Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mallard Creek Polymers Rovene® 6201 Styrene-Acrylic Resin

Category Polymer , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers Rovene® 6201 Styrene-Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Rovene® 6201 is an alkali soluble styrene-acrylic resin with a mid-range molecular weight supplied in a clear pellet form. Rovene® 6201 is a general use resin for overprint varnishes, water based inks and pigment dispersions. Rovene® 6201 provides excellent ink transfer and printability with high gloss. Solution Preparation and Properties: The following are offered as starting point formulations. The resin should be cut under agitation and although Rovene® 6201 will dissolve at room temperature, the dissolution process can be greatly accelerated by the use of heat, up to 70°C. Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6201 Material Safety Data Sheet before handling, storing, or using this product.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0407 lb/in³
Volatiles <= 2.0 %
<= 2.0 %
Molecular Weight 7000 g/mol
7000 g/mol
Thermal Properties Metric English Comments
Softening Point 155 °C
311 °F
Glass Transition Temp, Tg 120 °C
248 °F
Chemical Properties Metric English Comments
Total Acid Number 218
218
[mgKOH/g]