MetalTek MTEK 27-5 Cast UNS J93015 Heat Resistant Stainless Steel

Category Metal , Ferrous Metal , Heat Resisting , Stainless Steel , Cast Stainless Steel
Manufacturer MetalTek
Trade Name MTEK
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF MetalTek MTEK 27-5 Cast UNS J93015 Heat Resistant Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Higher nickel yields improved strength. Resists high sulfur process gas.Applications: Pour spouts, holding pots, kiln parts, gas parts.Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 192
192
Tensile Strength, Ultimate >= 515 MPa
>= 74700 psi
Tensile Strength, Yield >= 240 MPa
>= 34800 psi
Elongation at Break >= 8.0 %
>= 8.0 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 700 °C
1290 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.50 %
<= 0.50 %
Chromium, Cr 26 - 30 %
26 - 30 %
Iron, Fe 59 - 70 %
59 - 70 %
As Balance
Manganese, Mn <= 1.5 %
<= 1.5 %
Nickel, Ni 4.0 - 7.0 %
4.0 - 7.0 %
Silicon, Si <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Heat Treatment Not Heat Treated