Michelman® Hydrosize® U2022 Nonionic polyurethane emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Michelman®
Trade Name Hydrosize®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Hydrosize® U2022 Nonionic polyurethane emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2022 is an APE free, high strength sizing for glass and carbon chopped fiber, with excellent adhesion.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.15 g/cc
1.00 - 1.15 g/cc
Volatiles 40 - 42 %
40 - 42 %
pH 6.5 - 8.5
6.5 - 8.5
Brookfield Viscosity 500 - 1700 cP
500 - 1700 cP
Spindle # 3, rpm 60
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength 34.5 - 48.3 MPa
5000 - 7000 psi
Elongation at Break 700 %
700 %
100% Modulus 0.000200 - 0.000221 GPa
0.0290 - 0.0320 ksi
Descriptive Properties Value Comments
Appearance Milky white
Emulsifier Charge Anionic/Nonionic
Solids Type Polyurethane