Microcell Composite Company CELLOMER® 2100D SBS Rubber Pellets

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Microcell Composite Company
Trade Name CELLOMER®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Microcell Composite Company CELLOMER® 2100D SBS Rubber Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CELLOMER® PELLETS can be used in hot-pressing or with injection foaming boards. Featuring anti-slippage and elasticity.Information provided by Microcell Composite Company
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Melt Flow 1.365 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.365 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 59
59
Tensile Strength, Yield 5.582 MPa
809.6 psi
Elongation at Yield 607 %
607 %
Tear Strength 24.60 kN/m
140.5 pli