Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials HV 3/706 Heat Cured Rubber - High Temperature

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials HV 3/706 Heat Cured Rubber - High Temperature.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.HV 3/706 is a specialty grade, peroxide curable silicone elastomer.Key Feature: Heat resistance up to 300°C
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength 10.0 MPa
1450 psi
Elongation at Break 350 %
350 %
Tear Strength 20.0 kN/m
114 pli
Die B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Optical Properties Metric English Comments
Transmission, Visible 20 %
20 %
translucent; thickness unknown
Descriptive Properties Value Comments
Appearance Translucent
Users viewing this material also viewed the following: