Momentive Performance Materials TSE399 Translucent Adhesive Sealant, Flowable

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials TSE399 Translucent Adhesive Sealant, Flowable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Non-corrosive adhesive/sealant/coating for metallic and plastics substrates; for electrical/electronic applications.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Tensile Strength, Ultimate 13.0 MPa
1890 psi
Elongation at Break 140 %
140 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 205 °C
401 °F
Continuous useful temperature.
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Continuous useful temperature.
Electrical Properties Metric English Comments
Dielectric Constant 2.9
2.9
Dielectric Strength 20.0 kV/mm
508 kV/in
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F