| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792-91 |
| Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | ASTM D955-89 |
| Melt Flow | 3.3 g/10 min | 3.3 g/10 min | (Condition I) ASTM D-1238-94a |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 103 | 103 | ASTM D785-95 |
| Tensile Strength, Ultimate | 50.0 MPa | 7250 psi | ASTM D638-95 |
| Elongation at Break | 40 % | 40 % | ASTM D638-95 |
| Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790-95 |
| Flexural Modulus | 2.483 GPa | 360.1 ksi | RT; ASTM D-790-95 |
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256-93a |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C | 194 °F | ASTM D648-95 |
| Vicat Softening Point | 110 °C | 230 °F | ASTM D1525-95 |
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |
|
| HB @Thickness 3.17 mm |
HB @Thickness 0.125 in |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Gloss | 82 - 90 % | 82 - 90 % | ASTM D2457-90 |