Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Pro® 1602 S Black Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Multibase
Trade Name Multi-Pro®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 1602 S Black Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792-91
Melt Flow 12 g/10 min
12 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638-95
Elongation at Break 570 %
570 %
ASTM D638-95
Flexural Modulus 1.379 GPa
200.0 ksi
ASTM D790-95
Gardner Impact 3.40 J
2.51 ft-lb
ASTM D5420-93