Material Notes:
NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consider. Applications include Aerospace, Automotive, Chemical, Food, Industrial, Pharmaceutical, Semiconductor, Nuclear, and Oil & Gas.
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 85

@Thickness 6.00 mm
75 - 85

@Thickness 0.236 in
DIN 53505
Tensile Strength >= 18.0 MPa
>= 2610 psi
DIN 53504
Elongation at Break >= 110 %
>= 110 %
DIN 53504
100% Modulus >= 0.00400 GPa
>= 0.580 ksi
DIN 53504
Compression Set <= 25 %

@Temperature 200 °C,
Time 259000 sec
<= 25 %

@Temperature 392 °F,
Time 72.0 hour
DIN 53517
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Descriptive Properties Value Comments
Color White