| Category | Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS) |
| Manufacturer | NOVA Chemicals |
| Trade Name | EPS |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | NOVA Chemicals EPS 33MAHD Modified Expandable Polystyrene.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Double Pass Continuous Expansion |
| >= 0.0160 g/cc | >= 0.000579 lb/in³ | Batch Expansion | |
| >= 0.0224 g/cc | >= 0.000810 lb/in³ | Single Pass Continuous Expansion |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Bead Size | 1.4 mm | Unexpanded |
| Pentane | 5.3 wt% |