Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® 8504 UV8D, 8504G UV8D MDPE Rotational Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 8504 UV8D, 8504G UV8D MDPE Rotational Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Low melt index, excellent ESCR, high toughness at low temperatures.Applications: Large chemical storage tanks.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
F50, Condition A, ASTM D1693, 100% Igepal
Melt Flow 1.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ASTM D2240
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM D638
Elongation at Break >= 1000 %
>= 1000 %
ASTM D638
Flexural Modulus 0.650 GPa
94.3 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 118 °C
244 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 170 - 215 °C