| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled |
| Manufacturer | Niche Polymer |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Niche Polymer PA6GF33N Nylon 6, 33% Glass Fiber Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.00250 cm/cm | 0.00250 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 159 MPa | 23000 psi | ASTM D638 |
| Elongation at Break | 3.50 % | 3.50 % | ASTM D638 |
| Flexural Strength | 200 MPa | 29000 psi | ASTM D790 |
| Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
| Izod Impact, Unnotched | 1.12 J/cm @Thickness 3.17 mm |
2.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 216 - 228 °C | 420 - 442 °F | ASTM D789 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Natural |