| Category | Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Wood Filled |
| Manufacturer | North Wood Plastics |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | North Wood Plastics HDPE with 60% Wood Fiber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.158 g/cc | 0.04184 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0056 cm/cm | 0.0056 in/in | ASTM D955 |
| Melt Flow | 1.5 g/10 min @Temperature 190 °C |
1.5 g/10 min @Temperature 374 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | ASTM D638 |
| Tensile Strength, Yield | 16.0 MPa | 2320 psi | ASTM D638 |
| Elongation at Break | 1.3 % | 1.3 % | ASTM D638 |
| Tensile Modulus | 4.40 GPa | 638 ksi | ASTM D638 |
| Flexural Yield Strength | 30.0 MPa | 4350 psi | ASTM D790 |
| Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
| Izod Impact, Unnotched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 36.0 µm/m-°C @Temperature 20.0 °C |
20.0 µin/in-°F @Temperature 68.0 °F |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
| Flammability, UL94 | HB | HB | 0.32 cm x 1.25 cm x 12.5 cm sample |
| HB | HB | 0.32 cm x 1.25 cm x 12.5 cm sample |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | <= 200 °C | <= 392 °F | To prevent fiber degradation. |