Material Notes:
Arnite is a relatively new semi-crystalline polymer developed for technical applications. It is suitable for mechanical parts which require dimensional stability and a low friction coefficient. Omnialite is a modified PET designed to provide a higher shock resistance than Arnite by reducing the E-modulus.Features:Low friction coefficientDimensional stability both at temperature and humidityCompressive strength even at low temperatureExcellent machinabilityHigh fatigue resistanceColour: naturalWeak Point:The material is very stiff so the shock resistance is not high. It is possible to modify it with the addition of other polymers but this operation is done to the detriment of such characteristics as stiffness, compressive and flexural strength which are the typical features of PET.Application:Mechanical: thanks to its low friction coefficient it is particularly suitable for sliding blocks, slide ways, bearings, guides, etc. Its dimensional stability makes it an excellent choice for precision parts where tight tolerances must be maintained both in moist and hot conditions.Food contact: it is physiological inert and extensively used in the food industry.Electrical: the excellent electrical features (stable in the long run) make PET suitable for insulators and other electrical components.Chemical: good resistance to acids and chlorine solutions.Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO.1183 DIN.53479
Moisture Absorption at Equilibrium 0.20 %
0.20 %
50% relative humidity
Water Absorption at Saturation 0.50 %
0.50 %
23°C
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
dry sample; ISO2039.2
Ball Indentation Hardness 170 MPa
24700 psi
ISO2039.1 DIN.53456
Tensile Strength at Break 85.0 MPa
12300 psi
ISO.527 DIN.53455
Elongation at Break 50 %
50 %
ISO.527 DIN.53455
Tensile Modulus 3.10 GPa
450 ksi
ISO.527 DIN.53455
Compressive Strength 20.0 MPa
2900 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched NB
NB
7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO179/3C DIN.53453
Coefficient of Friction, Dynamic 0.25
0.25
on dry ground steel; load =0.05MPa; speed =0.6 m/s
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 140 °F
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
DIN.52612
Melting Point 255 °C
491 °F
Maximum Service Temperature, Air 115 °C
239 °F
Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C.
170 °C
338 °F
short period, no load
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ISO.75 DIN.53461
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
impact conditions and heavy loads not considered
Flammability, UL94 HB
HB
Oxygen Index 22 %
22 %
ISO.4589
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ISO.93 DIN.53482
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
ISO.250 DIN.53483
Dielectric Strength 60.0 kV/mm
1520 kV/in
ISO.243 DIN.53481
Dissipation Factor 0.010

@Frequency 1e+6 Hz
0.010

@Frequency 1e+6 Hz
ISO.250 DIN.53483