Material Notes:
Dry as molded. Injection molding grade. Nylene 452 is a plasticized, injection molding nylon for use in applications requiring high flexibility, and excellent toughness and abrasion resistance. Because of its internal lubricant and high monomer content, Nylene 452 will perform well in critical molding processes requiring very good melt flow.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Water Absorption 3.9 %
3.9 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 360 %
360 %
ASTM D638
Flexural Yield Strength 44.0 MPa
6380 psi
ASTM D790
Izod Impact, Notched 1.90 J/cm
3.56 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
306 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ASTM D495
Processing Properties Metric English Comments
Processing Temperature 232 - 243 °C
450 - 469 °F
At Nozzle
Nozzle Temperature 232 - 243 °C
450 - 469 °F