Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Omni Plastics OmniLon™ 6/6 PA6/6 GR20 IM10 Glass Reinforced/Impact Modified Nylon

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Omni Plastics
Trade Name OmniLon™ 6/6
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omni Plastics OmniLon™ 6/6 PA6/6 GR20 IM10 Glass Reinforced/Impact Modified Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
Flexural Modulus 5.96 GPa
865 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm
2.80 ft-lb/in
ASTM D256