Osprey Metals HTN 4 Brazing Powder

Category Metal , Nonferrous Metal , Nickel Alloy , Solder/Braze Alloy
Manufacturer Osprey Metals, Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Osprey Metals HTN 4 Brazing Powder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requirements.The specifications listed are subject to the benefits and scrutiny of Osprey's accreditation to ISO 9001. If the product delivered does not substantially meet the specification, Osprey will replace it. Osprey's liability is limited to the cost of replacement. Information provided to MatWeb by Osprey Metals.
Thermal Properties Metric English Comments
Melting Point 980 - 1070 °C
1800 - 1960 °F
Solidus 980 °C
1800 °F
Liquidus 1070 °C
1960 °F
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.050 %
<= 0.050 %
Boron, B 1.5 - 2.2 %
1.5 - 2.2 %
Carbon, C <= 0.060 %
<= 0.060 %
Cobalt, Co <= 0.10 %
<= 0.10 %
Iron, Fe <= 1.5 %
<= 1.5 %
Nickel, Ni 94.6 %
94.6 %
Other <= 0.50 %
<= 0.50 %
Oxygen, O >= 0.025 %
>= 0.025 %
Phosphorous, P <= 0.020 %
<= 0.020 %
Selenium, Se <= 0.0050 %
<= 0.0050 %
Silicon, Si 3.0 - 4.0 %
3.0 - 4.0 %
Sulfur, S <= 0.020 %
<= 0.020 %
Titanium, Ti <= 0.050 %
<= 0.050 %
Zirconium, Zr <= 0.050 %
<= 0.050 %