| Category | Metal , Ferrous Metal , Austenitic , Stainless Steel |
| Manufacturer | Outokumpu |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Outokumpu 4318 Cr-Ni Austenitic Stainless Steel.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 7.90 g/cc | 0.285 lb/in³ | RT |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 765 MPa | 111000 psi | Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1 |
| 440 MPa @Temperature 300 °C |
63800 psi @Temperature 572 °F |
EN min.; EN 10002-5 | |
| 460 MPa @Temperature 200 °C |
66700 psi @Temperature 392 °F |
EN min.; EN 10002-5 | |
| 530 MPa @Temperature 100 °C |
76900 psi @Temperature 212 °F |
EN min.; EN 10002-5 | |
| Tensile Strength, Yield | 350 MPa @Strain 0.200 % |
50800 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
| 360 MPa @Strain 0.200 % |
52200 psi @Strain 0.200 % |
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1 | |
| 395 MPa @Strain 1.00 % |
57300 psi @Strain 1.00 % |
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1 | |
| 170 MPa @Strain 0.200 %, Temperature 300 °C |
24700 psi @Strain 0.200 %, Temperature 572 °F |
EN min.; EN 10002-5 | |
| 185 MPa @Strain 0.200 %, Temperature 200 °C |
26800 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 | |
| 200 MPa @Strain 1.00 %, Temperature 300 °C |
29000 psi @Strain 1.00 %, Temperature 572 °F |
EN min.; EN 10002-5 | |
| 215 MPa @Strain 1.00 %, Temperature 200 °C |
31200 psi @Strain 1.00 %, Temperature 392 °F |
EN min.; EN 10002-5 | |
| 265 MPa @Strain 0.200 %, Temperature 100 °C |
38400 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 | |
| 300 MPa @Strain 1.00 %, Temperature 100 °C |
43500 psi @Strain 1.00 %, Temperature 212 °F |
EN min.; EN 10002-5 | |
| Elongation at Break | 47 % | 47 % | Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1 |
| Modulus of Elasticity | 200 GPa | 29000 ksi | RT |
| 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
||
| 172 GPa @Temperature 400 °C |
24900 ksi @Temperature 752 °F |
||
| 179 GPa @Temperature 300 °C |
26000 ksi @Temperature 572 °F |
||
| 186 GPa @Temperature 200 °C |
27000 ksi @Temperature 392 °F |
||
| 194 GPa @Temperature 100 °C |
28100 ksi @Temperature 212 °F |
||
| Poissons Ratio | 0.30 | 0.30 | RT |
| Shear Modulus | 77.0 GPa | 11200 ksi | calculated |
| Impact Test | >= 60.0 J | >= 44.3 ft-lb | Hot rolled plate/Cold rolled strip/sheet, 10x10mm test pieces; EN 10045-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 16.0 µm/m-°C @Temperature 100 °C |
8.89 µin/in-°F @Temperature 212 °F |
|
| 16.5 µm/m-°C @Temperature 200 °C |
9.17 µin/in-°F @Temperature 392 °F |
||
| 17.0 µm/m-°C @Temperature 300 °C |
9.44 µin/in-°F @Temperature 572 °F |
||
| 17.5 µm/m-°C @Temperature 400 °C |
9.72 µin/in-°F @Temperature 752 °F |
||
| 18.0 µm/m-°C @Temperature 500 °C |
10.0 µin/in-°F @Temperature 932 °F |
||
| Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | RT |
| Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
| 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Carbon, C | 0.020 % | 0.020 % | |
| Chromium, Cr | 17.7 % | 17.7 % | |
| Iron, Fe | 75.64 % | 75.64 % | |
| Nickel, Ni | 6.5 % | 6.5 % | |
| Nitrogen, N | 0.14 % | 0.14 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000730 ohm-cm | 0.0000730 ohm-cm | RT |