| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 7.70 g/cc | 0.278 lb/in³ | RT |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 805 MPa | 117000 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
| Tensile Strength, Yield | 507 MPa @Strain 0.200 % |
73500 psi @Strain 0.200 % |
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
| 530 MPa @Strain 0.200 % |
76900 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 | |
| 400 MPa @Strain 0.200 %, Temperature 200 °C |
58000 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 | |
| 450 MPa @Strain 0.200 %, Temperature 100 °C |
65300 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 | |
| Elongation at Break | 35 % | 35 % | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
| Modulus of Elasticity | 200 GPa | 29000 ksi | RT |
| 172 GPa @Temperature 400 °C |
24900 ksi @Temperature 752 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 13.0 µm/m-°C @Temperature 100 °C |
7.22 µin/in-°F @Temperature 212 °F |
|
| 14.5 µm/m-°C @Temperature 400 °C |
8.06 µin/in-°F @Temperature 752 °F |
||
| Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | RT |
| Thermal Conductivity | 15.0 W/m-K | 104 BTU-in/hr-ft²-°F | RT |
| 20.0 W/m-K @Temperature 400 °C |
139 BTU-in/hr-ft²-°F @Temperature 752 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Carbon, C | 0.020 % | 0.020 % | |
| Chromium, Cr | 25 % | 25 % | |
| Copper, Cu | 0.50 % | 0.50 % | |
| Iron, Fe | 62.91 % | 62.91 % | |
| Molybdenum, Mo | 3.8 % | 3.8 % | |
| Nickel, Ni | 7.0 % | 7.0 % | |
| Nitrogen, N | 0.27 % | 0.27 % | |
| Tungsten, W | 0.50 % | 0.50 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000800 ohm-cm | 0.0000800 ohm-cm | RT |