Material Notes:
Nylon 6 - Glass reinforced (43 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the measurements are done in dry and wet conditions. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm

@Thickness 3.17 mm
0.0010 - 0.0020 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 140 MPa
20300 psi
50 mm/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
50 mm/min; ASTM D638
Tensile Modulus 5.70 GPa
827 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 180 MPa
26100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
1.3 mm/min; ASTM D790