| Category | Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Overview of materials for Thermoset Polyurethane Foam, Unreinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.0250 - 1.39 g/cc | 0.000903 - 0.0504 lb/in³ | Average value: 0.407 g/cc Grade Count:149 |
| Apparent Bulk Density | 0.0220 - 0.880 g/cc | 0.000795 - 0.0318 lb/in³ | Average value: 0.262 g/cc Grade Count:24 |
| Water Absorption | 0.700 - 38.0 % | 0.700 - 38.0 % | Average value: 9.14 % Grade Count:56 |
| Moisture Absorption at Equilibrium | 2.00 % | 2.00 % | Average value: 2.00 % Grade Count:16 |
| Water Absorption at Saturation | 5.00 - 20.0 % | 5.00 - 20.0 % | Average value: 12.3 % Grade Count:11 |
| Thickness | 27.9 - 12700 microns | 1.10 - 500 mil | Average value: 2230 microns Grade Count:26 |
| Linear Mold Shrinkage | 0.000800 - 0.0100 cm/cm | 0.000800 - 0.0100 in/in | Average value: 0.00627 cm/cm Grade Count:9 |
| Outgassing - Total Mass Loss | 0.0400 - 1.73 % @Temperature 125 - 125 °C |
0.0400 - 1.73 % @Temperature 257 - 257 °F |
Average value: 0.609 % Grade Count:14 |
| 0.0400 - 1.73 % @Time 86400 - 86400 sec |
0.0400 - 1.73 % @Time 24.0 - 24.0 hour |
Average value: 0.609 % Grade Count:14 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 3.00 - 60.0 | 3.00 - 60.0 | Average value: 26.6 Grade Count:36 |
| Hardness, Shore D | 28.0 - 81.0 | 28.0 - 81.0 | Average value: 57.1 Grade Count:11 |
| Hardness, Shore O | 2.00 - 65.0 | 2.00 - 65.0 | Average value: 27.6 Grade Count:34 |
| Hardness, Shore OO | 10.0 - 45.0 | 10.0 - 45.0 | Average value: 30.8 Grade Count:4 |
| Tensile Strength, Ultimate | 0.0827 - 1900 MPa | 12.0 - 276000 psi | Average value: 42.8 MPa Grade Count:111 |
| Tensile Strength, Yield | 0.241 - 103 MPa | 35.0 - 15000 psi | Average value: 30.3 MPa Grade Count:43 |
| Film Elongation at Break, MD | 78.0 % | 78.0 % | Average value: 78.0 % Grade Count:6 |
| 74.0 - 74.0 % @Temperature 66.0 - 66.0 °C |
74.0 - 74.0 % @Temperature 151 - 151 °F |
Average value: 74.0 % Grade Count:6 | |
| 74.0 - 74.0 % @Time 346000 - 346000 sec |
74.0 - 74.0 % @Time 96.0 - 96.0 hour |
Average value: 74.0 % Grade Count:6 | |
| Film Elongation at Break, TD | 32.0 % | 32.0 % | Average value: 32.0 % Grade Count:6 |
| 66.0 - 66.0 % @Temperature 66.0 - 66.0 °C |
66.0 - 66.0 % @Temperature 151 - 151 °F |
Average value: 66.0 % Grade Count:6 | |
| 66.0 - 66.0 % @Time 346000 - 346000 sec |
66.0 - 66.0 % @Time 96.0 - 96.0 hour |
Average value: 66.0 % Grade Count:6 | |
| Elongation at Break | 3.20 - 760 % | 3.20 - 760 % | Average value: 161 % Grade Count:116 |
| Modulus of Elasticity | 0.000138 - 3.45 GPa | 0.0200 - 500 ksi | Average value: 1.39 GPa Grade Count:36 |
| Flexural Yield Strength | 6.60 - 62.0 MPa | 957 - 8990 psi | Average value: 23.6 MPa Grade Count:17 |
| Flexural Modulus | 0.0165 - 1.93 GPa | 2.40 - 280 ksi | Average value: 0.857 GPa Grade Count:16 |
| Compressive Yield Strength | 0.00172 - 48.0 MPa | 0.250 - 6960 psi | Average value: 2.16 MPa Grade Count:134 |
| Compressive Modulus | 0.0000276 - 1.15 GPa | 0.00400 - 167 ksi | Average value: 0.0996 GPa Grade Count:34 |
| Resilience | 29.0 - 52.0 | 29.0 - 52.0 | Average value: 38.8 Grade Count:13 |
| Rebound | 19.0 - 31.0 % | 19.0 - 31.0 % | Average value: 25.5 % Grade Count:6 |
| Poissons Ratio | 0.300 - 0.750 | 0.300 - 0.750 | Average value: 0.353 Grade Count:8 |
| Shear Modulus | 0.00122 - 0.870 GPa | 0.177 - 126 ksi | Average value: 0.0729 GPa Grade Count:16 |
| Shear Strength | 0.110 - 16.0 MPa | 16.0 - 2320 psi | Average value: 3.10 MPa Grade Count:16 |
| Charpy Impact, Notched | 0.380 - 3.20 J/cm² | 1.81 - 15.2 ft-lb/in² | Average value: 1.43 J/cm² Grade Count:9 |
| Coefficient of Friction | 0.400 - 1.40 | 0.400 - 1.40 | Average value: 0.463 Grade Count:16 |
| Tear Strength Test | 30.0 - 137 | 30.0 - 137 | Average value: 84.6 Grade Count:13 |
| Tear Strength | 0.0400 - 10.5 kN/m | 0.228 - 60.0 pli | Average value: 1.08 kN/m Grade Count:71 |
| Peel Strength | 0.438 - 0.892 kN/m | 2.50 - 5.09 pli | Average value: 0.648 kN/m Grade Count:6 |
| Compression Set | 1.30 - 54.0 % | 1.30 - 54.0 % | Average value: 8.23 % Grade Count:68 |
| 0.000 - 35.0 % @Temperature 70.0 - 125 °C |
0.000 - 35.0 % @Temperature 158 - 257 °F |
Average value: 8.36 % Grade Count:57 | |
| <= 10.0 % @Temperature 70.0 - 70.0 °C |
<= 10.0 % @Temperature 158 - 158 °F |
Average value: 8.36 % Grade Count:1 | |
| <= 10.0 % @Time 79200 - 79200 sec |
<= 10.0 % @Time 22.0 - 22.0 hour |
Average value: 8.36 % Grade Count:1 | |
| Seal Strength | 9.40 g/25 mm | 9.40 g/in | Average value: 9.40 g/25 mm Grade Count:6 |
| 10.6 - 10.6 g/25 mm @Temperature 66.0 - 66.0 °C |
10.6 - 10.6 g/in @Temperature 151 - 151 °F |
Average value: 10.6 g/25 mm Grade Count:6 | |
| 10.6 - 10.6 g/25 mm @Time 346000 - 346000 sec |
10.6 - 10.6 g/in @Time 96.0 - 96.0 hour |
Average value: 10.6 g/25 mm Grade Count:6 | |
| Film Tensile Strength at Break, MD | 207 MPa | 30000 psi | Average value: 207 MPa Grade Count:3 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 63.0 - 310 µm/m-°C | 35.0 - 172 µin/in-°F | Average value: 214 µm/m-°C Grade Count:39 |
| Thermal Conductivity | 0.0760 - 0.830 W/m-K | 0.527 - 5.76 BTU-in/hr-ft²-°F | Average value: 0.129 W/m-K Grade Count:17 |
| Insulation R Value | 5.20 - 6.00 | 5.20 - 6.00 | Average value: 5.60 Grade Count:4 |
| Maximum Service Temperature, Air | 70.0 - 149 °C | 158 - 300 °F | Average value: 99.5 °C Grade Count:57 |
| Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 100 °C | 117 - 212 °F | Average value: 77.4 °C Grade Count:7 |
| Minimum Service Temperature, Air | -183 - 121 °C | -297 - 250 °F | Average value: 38.1 °C Grade Count:27 |
| Brittleness Temperature | -51.0 - -12.0 °C | -59.8 - 10.4 °F | Average value: -36.5 °C Grade Count:24 |
| Flammability, UL94 | HB - 5VA | HB - 5VA | Grade Count:10 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90.0 % | 90.0 % | Average value: 90.0 % Grade Count:5 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 3.00e+10 - 3.20e+14 ohm-cm | 3.00e+10 - 3.20e+14 ohm-cm | Average value: 4.19e+13 ohm-cm Grade Count:38 |
| Surface Resistance | 0.100 - 1.00e+15 ohm | 0.100 - 1.00e+15 ohm | Average value: 1.08e+14 ohm Grade Count:23 |
| 0.00700 - 0.0170 ohm @Temperature 35.0 - 121 °C |
0.00700 - 0.0170 ohm @Temperature 95.0 - 250 °F |
Average value: 0.0105 ohm Grade Count:5 | |
| 0.00700 - 0.0170 ohm @Time 605000 - 7.88e+6 sec |
0.00700 - 0.0170 ohm @Time 168 - 2190 hour |
Average value: 0.0105 ohm Grade Count:5 | |
| Shielding Effectiveness | 62.0 - 110 dB | 62.0 - 110 dB | Average value: 87.5 dB Grade Count:8 |
| Dielectric Constant | 1.48 - 2.69 | 1.48 - 2.69 | Average value: 1.73 Grade Count:30 |
| Dielectric Strength | 1.65 - 13.8 kV/mm | 42.0 - 350 kV/in | Average value: 2.83 kV/mm Grade Count:39 |
| Dissipation Factor | 0.0400 - 0.0500 | 0.0400 - 0.0500 | Average value: 0.0485 Grade Count:27 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 21.1 - 60.0 °C | 70.0 - 140 °F | Average value: 28.9 °C Grade Count:14 |