Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oxford Polymers Oxnilon 66-15-IMP Impact Modified Nylon 66 for Injection Molding

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Oxford Polymers
Trade Name Oxnilon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers Oxnilon 66-15-IMP Impact Modified Nylon 66 for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Impact Modified Nylon 66 for Injection MoldingInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 51.7 MPa
7500 psi
ASTM D638
Elongation at Break 210 %
210 %
ASTM D638
Flexural Modulus 1.69 GPa
245 ksi
ASTM D790
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 282 - 293 °C
540 - 560 °F
Users viewing this material also viewed the following: