Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P(HT) Powdered Metal

Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel
Manufacturer PSM Industries
Trade Name Pacific Sintered Metals
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P(HT) Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FC-0208-50HTInformation Provided by Pacific Sintered Metals, a division of PSM Industries
Physical Properties Metric English Comments
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 20
20
Tensile Strength, Ultimate 448 MPa
65000 psi
Elongation at Break <= 1.0 %
<= 1.0 %
1 in. gauge
Flexural Strength 655 MPa
95000 psi
Transverse Rupture
Charpy Impact, Unnotched 4.07 J
3.00 ft-lb