Petromont 4101 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Petromont
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petromont 4101 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Petromont HDPE 4101 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is primarily used in the extrusion of corrugated pipes for drainage applications, for sewer pipes and for a wide range of profile extrusion applications. It has been specifically designed for corrugated pipes with the addition of colour concentrates.Petromont HDPE 4101 complies with the material requirements specified by AASHTO M 294. When mixed with an appropriate carbon black masterbatch, Petromont HDPE 4101 black meets the CSA B182.8 standard for use in profile storm sewer pipe and fabricated fittings.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
Melt Flow 0.22 g/10 min
0.22 g/10 min
I<sub>2</sub>; ASTM D1238
20 g/10 min
20 g/10 min
I<sub>21</sub>; ASTM D238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.2 MPa
3800 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Tensile Load, Notched Constant >= 24.0 hour
>= 24.0 hour
Single Point; ASTM D5397
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D746
Descriptive Properties Value Comments
Process Pipe Extrusion