Plaskolite West Optix® CA-51 General Purpose Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA-51 General Purpose Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Injection Molding and Extrusion Grade Pellets. Medium heat resistance and medium flow.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Melt Flow 15.5 g/10 min
15.5 g/10 min
Condition 230/2-8; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 56.0 MPa
8120 psi
ASTM D638
Elongation at Break 2.6 %
2.6 %
ASTM D638
Modulus of Elasticity 2.90 GPa
421 ksi
ASTM D638
Flexural Strength 102 MPa
14800 psi
ASTM D790
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
Gardner Impact 0.226 J
0.167 ft-lb
Falling Weight; ASTM D3029GB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C
169 °F
ASTM D648
Vicat Softening Point 94.0 °C
201 °F
ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 92 %
92 %
Luminous Transmittance, ASTM D1003