Plaskolite West Optix® CA-927 HF Clear Impact Modified Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Impact Modified, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA-927 HF Clear Impact Modified Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Impact modified acrylic resin, injection molding gradeApplications: A high flow, impact-modified acrylic resin for injection molding. This resin offers impact strengths up to seven times those of general-purpose acrylic resins and, at the same time, a high melt flow rate.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 49.6 MPa
7190 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Modulus of Elasticity 2.38 GPa
345 ksi
ASTM D638
Flexural Strength 48.3 MPa
7010 psi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Gardner Impact 3.16 J
2.33 ft-lb
Falling Weight; ASTM D3029GB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
163 °F
ASTM D648
Vicat Softening Point 108 °C
226 °F
Rate A, ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
ASTM D1003