Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastiComp Complet® LCF30-PC/ABS Polycarbonate/ABS Alloy, 30% Long Carbon Fiber Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Carbon Fiber Reinforced
Manufacturer PlastiComp
Trade Name Complēt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LCF30-PC/ABS Polycarbonate/ABS Alloy, 30% Long Carbon Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polycarbonate/ABS Alloy with 30% long carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D-792
Filler Content 30 %
30 %
Long Carbon Fiber
Mechanical Properties Metric English Comments
Tensile Strength 159 MPa
23100 psi
ASTM D-638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D-638
Tensile Modulus 15.172 GPa
2200.5 ksi
ASTM D-638
Flexural Strength 241 MPa
35000 psi
ASTM D-790
Flexural Modulus 26.283 GPa
3812.0 ksi
ASTM D-790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 7.48 J/cm
14.0 ft-lb/in
ASTM D-4812