Polimeri Europa Intex® 2740 Styrene - Butadiene Copolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Intex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Intex® 2740 Styrene - Butadiene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Intex® 2740 is an aqueous anionic dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain any antioxidant.Key Features: The vulcanized latex shows excellent mechanical properties. Intex® 2740 can be blended with natural latexMain Applications: Intex® 2740 is mainly used for very high stiffness molded foams obtained by both Dunlap and Talalay processes.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Solids Content 66 %
66 %
Total; ISO 124
pH 10.3
10.3
ISO 976
Brookfield Viscosity 1000 cP
1000 cP
60 rpm; ISO 1652
Chemical Properties Metric English Comments
Styrene Content 40 %
40 %
Bound; Internal method