Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Riblene® GP 26 Low Density Polyethylene - Coating Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Riblene® GP 26 Low Density Polyethylene - Coating Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Riblene GP 26 is a high fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GP 26 is suitable for coating applications where low neck-in and high draw-down are key factors. For its excellent organoleptic properties Riblene GP 26 can be used for foodstuff flexible packaging. Moreover, for its rheological properties, Riblene GP 26 can be used for injection molded medium thickness articles, toys and houseware.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.921 g/cc
0.921 g/cc
ISO 1183
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 46
46
ISO 868/A
Tensile Strength at Break 11.0 MPa
1600 psi
ISO 527
Tensile Strength, Yield 9.00 MPa
1310 psi
ISO 527
Elongation at Break 500 %
500 %
ISO 527
Thermal Properties Metric English Comments
Melting Point 108 °C
226 °F
Internal method
Vicat Softening Point 85.0 °C

@Load 1.00 kg
185 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746