Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 185 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
50 N - 50°C/h; ISO 306/B
Polimeri Europa Edistir R 321P Polystyrene
Medium impact polystyrene combining easy flow and high stiffness. For injection moulding of parts with low thickness and high rigidity. Designation: Thermoplastics ISO 2897-PS-I,M,083-12-04-30Applic..
Vicat Softening Point 85.0 °C
185 °F
Rate B/50; ISO 306
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.
Vicat Softening Point 85.0 °C
185 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific)
Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied..
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy  (discontinued **)
Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol..
Vicat Softening Point 85.0 °C
<br>@Load 1.00 kg
185 °F
<br>@Load 2.20 lb
ISO 306/A
Polimeri Europa Greenflex® FD 20 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 20 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Films produced with Greenflex FD 20 exhibit good optical properties, high impact resistance, tensile ..
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
LyondellBasell Petrothene® NA952000 Low Density Polyethylene
ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process..
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties. Good Optical Properties. Additives : No Additive Applications: Agricultural FilmCSA No. 25895-47-0Information provided by LG Chemical
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Lucky IF-870 Acrylic, High Flow Grade
High flow for thin-walled injection molded parts and parts with long flow paths. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistanc..
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
LyondellBasell Petrothene® NA831000 Low Density Polyethylene
ApplicationsPETROTHENE NA831-000 resin exhibits high stress crack resistance and low temperature brittleness. Typical applications include housewares, containers and industrial parts. Regulatory St..
Vicat Softening Point 85.0 °C
<br>@Load 5.00 kg
185 °F
<br>@Load 11.0 lb
LATI Laticonther 92 GR/65 PUR, 65% Graphite Reinforced
High thermal conductivity product based on Polyurethane (PUR). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria ..
Vicat Softening Point 85.1 °C
<br>@Load 5.00 kg
185 °F
<br>@Load 11.0 lb
Shandong Rike Chemical HELIâ„¢ HL-755 Weather-resistance Acrylic Impact Modifier (AIM)
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c..
Vicat Softening Point 85.0 °C
<br>@Load 5.10 kg
185 °F
<br>@Load 11.2 lb
120°C/h; ASTM D 1525
Styrolution PS 153A GPPS
Styrolution PS 153A is an antistatic modified, general purpose polystyrene grade with a good flow characteristic.AntistaticGood flow characteristicsInformation provided by Styrolution
Vicat Softening Point 85.0 °C
185 °F
B/50; ISO R306
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 85.0 °C
185 °F
B/50; ISO R306
Samsung Cheil Industries Starex® VE-1805 HIPS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 85.0 °C
185 °F
B/50; ISO R306
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 85.0 °C
185 °F
B/50; ISO R306
Samsung Cheil Industries Starex® VH-0810 ABS, Unreinforced FR
Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus..
Vicat Softening Point 85.0 °C
185 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP
PPE+PP blend. Suitable for painted exterior automotive applications.
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Lubrizol Estane® S180A Thermoplastic Polyurethane
Type: Estane® S180A is a Shore 83A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mi..
Vicat Softening Point 85.0 °C
185 °F
A50; DIN 53460
Lubrizol ESTANE® X4985 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Vicat Softening Point 85.0 °C
<br>@Load 5.10 kg
185 °F
<br>@Load 11.2 lb
50°C per hour; ISO 306B50
Total PS CPDS 819 Flame Retardant Polystyrene
POLYSTYRENE (PS) COMPOUND (CPDS) 819 is a high impact brominated flame retardant polystyrene. A combination of high flow and high heat stability gives excellent processability and reduced cycle tim..
Vicat Softening Point 85.0 °C
185 °F
A50; DIN 53460
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Vicat Softening Point 85.0 °C
185 °F
1kg load; ISO 306
Eastman Drystar 0113 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Eastman Eastman 1223 Copolyester
Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card..
Vicat Softening Point 85.0 °C
<br>@Load 5.00 kg
185 °F
<br>@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTAPROP HK 2540 T8 Polypropylene, 20% Mineral Filled
PP homo/copolymer 20% mineral fillerGood physical and mechanical propertiesInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 85.0 °C
185 °F
Loading 1, Rate A; ASTM D1525
Chevron Phillips Marlex® 1009 LDPE Injection Molding Resin
Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: Large housewaresTamper evident, snap-on capsFeminine hygiene appl..
Vicat Softening Point 85.0 °C
185 °F
50N; ISO 306
Denka TP-801 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Diamond Polymers NPP 60-763 Clear Amorphous Polyester Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Vicat Softening Point 85.0 °C
185 °F
49 N; ISO 306
A.D. Compound Adene NCZAG Copolymer 70% CaCO3 Filled Polypropylene
Information provided by A.D. Compound
Vicat Softening Point 85.0 - 107 °C
185 - 225 °F
Average value: 94.6 °C Grade Count:28
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum ..
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
NOVA Chemicals Sclair® 2111 LLDPE Injection Molding Resin &nbsp;(discontinued **)
Good processability, Excellent impact resistance, Excellent flexibility and freedom from warpageApplications: Automotive splash-guards, Large containers, Closures and lids for food applicationsAddit..
Copyright © lookpolymers.com All Rights Reserved