| Category | Polymer , Thermoplastic , Liquid Crystal Polymer (LCP) , Liquid Crystal Polymer (LCP), Carbon Fiber Filled |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
| Water Absorption | 0.035 % | 0.035 % | 24 hrs. ASTM D570 |
| Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm @Thickness 3.17 mm |
0.0010 - 0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 190 MPa | 27600 psi | ASTM D638 |
| Elongation at Break | 1.0 - 3.0 % | 1.0 - 3.0 % | ASTM D638 |
| Tensile Modulus | 27.6 GPa | 4000 ksi | ASTM D638 |
| Flexural Yield Strength | 255 MPa | 37000 psi | ASTM D790 |
| Flexural Modulus | 27.6 GPa | 4000 ksi | ASTM D790 |
| Izod Impact, Notched | 0.530 - 0.800 J/cm @Thickness 6.35 mm |
0.993 - 1.50 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 249 °C | 480 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00 - 100 ohm-cm | 1.00 - 100 ohm-cm | ASTM D257 |
| Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 288 - 316 °C | 550 - 601 °F | Stock |
| Mold Temperature | 93.0 - 121 °C | 199 - 250 °F | |
| Drying Temperature | 149 - 163 °C | 300 - 325 °F |