Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.650 - 0.800 J/cm | 1.22 - 1.50 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to.. |
|||
Izod Impact, Notched | 0.160 - 0.801 J/cm | 0.300 - 1.50 ft-lb/in | Average value: 0.349 J/cm Grade Count:17 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 0.350 - 0.800 J/cm @Temperature -40.0 - 0.000 °C |
0.656 - 1.50 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.531 J/cm Grade Count:6 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Notched | 0.267 - 0.801 J/cm | 0.500 - 1.50 ft-lb/in | Average value: 0.526 J/cm Grade Count:32 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Izod Impact, Notched | 0.374 - 0.801 J/cm | 0.700 - 1.50 ft-lb/in | Average value: 0.587 J/cm Grade Count:12 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.534 - 0.801 J/cm | 1.00 - 1.50 ft-lb/in | Average value: 0.661 J/cm Grade Count:21 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.320 - 0.801 J/cm | 0.600 - 1.50 ft-lb/in | Average value: 0.564 J/cm Grade Count:15 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Izod Impact, Notched | 0.530 - 0.800 J/cm @Thickness 6.35 mm |
0.993 - 1.50 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ ATH-000/05M Acetal Homopolymer - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.600 - 0.800 J/cm @Temperature -40.0 - 0.000 °C |
1.12 - 1.50 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.642 J/cm Grade Count:1 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Notched | 0.600 - 0.800 J/cm @Thickness 3.20 - 3.20 mm |
1.12 - 1.50 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 0.642 J/cm Grade Count:1 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Notched | 0.267 - 0.801 J/cm | 0.500 - 1.50 ft-lb/in | Average value: 0.617 J/cm Grade Count:14 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Izod Impact, Notched | 0.374 - 0.800 J/cm | 0.700 - 1.50 ft-lb/in | Average value: 0.527 J/cm Grade Count:4 |
Overview of materials for Polyamide-Imide, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 0.530 - 0.800 J/cm @Thickness 6.35 mm |
0.993 - 1.50 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.108 - 0.800 J/cm | 0.202 - 1.50 ft-lb/in | Average value: 0.345 J/cm Grade Count:18 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Izod Impact, Notched | 0.400 - 0.801 J/cm | 0.749 - 1.50 ft-lb/in | Average value: 0.586 J/cm Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched | 0.320 - 0.801 J/cm | 0.600 - 1.50 ft-lb/in | Average value: 0.686 J/cm Grade Count:7 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.374 - 0.801 J/cm | 0.700 - 1.50 ft-lb/in | Average value: 0.618 J/cm Grade Count:8 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched | 0.600 - 0.800 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.12 - 1.50 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Izod Impact, Notched | 0.534 - 0.801 J/cm @Temperature 22.8 °C |
1.00 - 1.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA1SP0019 Nylon 66/PPS Alloy, 20% Glass, 20% Mineral Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.737 - 0.801 J/cm | 1.38 - 1.50 ft-lb/in | ASTM D256 |
Cast Nylons Nycast® SLX Premium Bearing Grade Nylon Nycast® SLX closes the gap between static and dynamic coefficients of friction. Used in wear pads, bearing blocks, and other load-bearing slide applications.Data provided by the manufacturer, Cast.. |
|||
Izod Impact, Notched | 0.400 - 0.801 J/cm | 0.750 - 1.50 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Izod Impact, Notched | 0.587 - 0.801 J/cm | 1.10 - 1.50 ft-lb/in | ASTM D256 |
Aaron Industries AVPS M 100-2 Virgin Polystyrene Melt flow index may be specified. |
|||
Izod Impact, Notched | 0.641 - 0.801 J/cm | 1.20 - 1.50 ft-lb/in | ASTM D256 |
Aaron Industries AAROLENE® ARPS MI 100-2 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Izod Impact, Notched | 0.270 - 0.800 J/cm @Temperature -40.0 - -40.0 °C |
0.506 - 1.50 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.447 J/cm Grade Count:11 |
Overview of materials for Ethyl Cellulose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ethyl Cellulose, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched | 0.267 - 0.801 J/cm | 0.500 - 1.50 ft-lb/in | Average value: 0.493 J/cm Grade Count:9 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |
|||
Izod Impact, Notched | 0.374 - 0.800 J/cm | 0.700 - 1.50 ft-lb/in | Average value: 0.544 J/cm Grade Count:7 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.800 - 0.800 J/cm @Temperature -40.0 - -40.0 °C |
1.50 - 1.50 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.800 J/cm Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Izod Impact, Notched | 0.26695 - 0.800 J/cm @Temperature 0.000 - 0.000 °C |
0.50011 - 1.50 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.516 J/cm Grade Count:3 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.26695 - 0.800 J/cm @Diameter 6.35 - 6.35 mm |
0.50011 - 1.50 ft-lb/in @Diameter 0.250 - 0.250 in |
Average value: 0.516 J/cm Grade Count:3 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.220 - 0.801 J/cm | 0.412 - 1.50 ft-lb/in | Average value: 0.471 J/cm Grade Count:18 |
Overview of materials for Polypropylene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app.. |