| Category | Polymer , Thermoplastic , Nylon , Nylon 610 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Edgetek® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Edgetek® NI-10GF/000 Polyamide 610 (Nylon 610).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0040 cm/cm | 0.0040 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 82.7 MPa | 12000 psi | Type I, 5.1 mm/min; ASTM D638 |
| Elongation at Break | 4.0 % | 4.0 % | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
| Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
| Izod Impact, Notched | 0.530 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 282 °C | 540 °F | |
| Mold Temperature | 93.3 °C | 200 °F | |
| Drying Temperature | 93.3 °C | 200 °F | |
| Dry Time | 4.00 hour | 4.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Filler / Reinforcement | Glass Fiber Reinforcement | |
| Forms | Pellets | |
| Generic Material | Nylon 610 | |
| Generic Name | Polyamide 610 (Nylon 610) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |