| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible 86479 Opaque Polyvinyl Chloride.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 76 | 76 | 15 sec; ASTM D2240 |
| 84 | 84 | ASTM D2240 | |
| Tensile Strength at Break | 16.5 MPa | 2390 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 7.58 MPa @Strain 100 % |
1100 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 390 % | 390 % | 510 mm/min; ASTM D638 |
| Tear Strength | 61.3 kN/m | 350 pli | Die C, 510 mm/min; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 179 - 188 °C | 354 - 370 °F | |
| 191 - 202 °C | 376 - 396 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Biocide | |
| UV Stabilizer | ||
| Features | High Gloss | |
| UV Absorbing | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Construction Applications | |
| Film | ||
| Sheet |