| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible A5D00 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.26 g/cc | 1.26 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 42 | 42 | 15 sec; ASTM D2240 |
| 55 | 55 | ASTM D2240 | |
| Tensile Strength at Break | 20.7 MPa | 3000 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 15.2 MPa @Strain 100 % |
2200 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 340 % | 340 % | 510 mm/min; ASTM D638 |
| Tear Strength | 118 kN/m | 673 pli | Die C, 510 mm/min; ASTM D624 |
| Compression Set | 62 % @Temperature 23.0 °C, Time 79200 sec |
62 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
| Clash Berg Modulus | 0.800 GPa | 116 ksi | ASTM D1043 |
| 0.310 GPa @Temperature -11.0 °C |
45.0 ksi @Temperature 12.2 °F |
ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -21.1 °C | -5.98 °F | ASTM D746 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 4.0 % @Thickness 1.91 mm |
4.0 % @Thickness 0.0750 in |
ASTM D1003 |
| Transmission, Visible | 75 % @Thickness 1.91 mm |
75 % @Thickness 0.0750 in |
ASTM D1003 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
| 193 - 204 °C | 379 - 399 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Clear/Transparent | |
| Features | General Purpose | |
| High Gloss | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Film | |
| General Purpose | ||
| Sheet |