| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible B65U0 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 57 | 57 | 15 sec; ASTM D2240 |
| 65 | 65 | ASTM D2240 | |
| Tensile Strength at Break | 10.3 MPa | 1490 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 3.62 MPa @Strain 100 % |
525 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 460 % | 460 % | 510 mm/min; ASTM D638 |
| Tear Strength | 38.5 kN/m | 220 pli | Die C, 510 mm/min; ASTM D624 |
| Compression Set | 22 % @Temperature 23.0 °C, Time 79200 sec |
22 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
| Clash Berg Modulus | 0.0241 GPa | 3.50 ksi | ASTM D1043 |
| 0.310 GPa @Temperature -55.0 °C |
45.0 ksi @Temperature -67.0 °F |
ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -51.1 °C | -60.0 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
| 188 - 199 °C | 370 - 390 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | UV Stabilizer | |
| Appearance | Opaque | |
| Features | Medium Gloss | |
| UV Absorbing | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |