| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible B6DB1 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 55 | 55 | 15 sec; ASTM D2240 |
| 60 | 60 | ASTM D2240 | |
| Tensile Strength at Break | 20.7 MPa | 3000 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 15.9 MPa @Strain 100 % |
2310 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 320 % | 320 % | 510 mm/min; ASTM D638 |
| Tear Strength | 105 kN/m | 599 pli | Die C, 510 mm/min; ASTM D624 |
| Clash Berg Modulus | 1.09 GPa | 158 ksi | ASTM D1043 |
| 0.310 GPa @Temperature -14.0 °C |
45.0 ksi @Temperature 6.80 °F |
ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -17.2 °C | 1.04 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
| 193 - 204 °C | 379 - 399 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Biocide | |
| Features | Medium Gloss | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |