Material Notes:
A flexible Vinyl compound for hose and tubing applications with enhanced physical characteristics.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 81
81
15 sec; ASTM D2240
87
87
ASTM D2240
Tensile Strength at Break 17.4 MPa
2520 psi
510 mm/min; ASTM D638
Tensile Strength 8.83 MPa

@Strain 100 %
1280 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 400 %
400 %
510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -34.4 °C
-29.9 °F
ASTM D746
Oxygen Index 23 %

@Thickness 1.57 mm
23 %

@Thickness 0.0618 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 179 - 185 °C
354 - 365 °F
Descriptive Properties Value Comments
Features General Purpose
Medium Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose