| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 65 | 65 | 15 sec; ASTM D2240 |
| 70 | 70 | ASTM D2240 | |
| Tensile Strength at Break | 9.65 MPa | 1400 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 4.14 MPa @Strain 100 % |
600 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 400 % | 400 % | 510 mm/min; ASTM D638 |
| Tear Strength | 28.0 kN/m | 160 pli | Die C, 510 mm/min; ASTM D624 |
| Clash Berg Modulus | 0.0662 GPa | 9.60 ksi | ASTM D1043 |
| 0.310 GPa @Temperature -43.0 °C |
45.0 ksi @Temperature -45.4 °F |
ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 168 - 177 °C | 334 - 351 °F | |
| 188 - 199 °C | 370 - 390 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | NSF 51 | BLACK 2999, NATURAL. Max. Temp. of use = 100 degrees F. |
| Features | Good Adhesion | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Coextrusion | |
| Extrusion | ||
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Construction Applications | |
| Seals | ||
| Weatherstripping |