Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Flexible P484 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible P484 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
15 sec; ASTM D2240
Tensile Strength at Break 20.7 MPa
3000 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 14.3 MPa

@Strain 100 %
2070 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 280 %
280 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 96.3 kN/m
549 pli
Die C, 510 mm/min; ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 177 - 182 °C
351 - 360 °F
193 - 204 °C
379 - 399 °F
Descriptive Properties Value Comments
Appearance Clear/Transparent
Features High Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Profile Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Furniture
Hose
Profiles
Tubing
Users viewing this material also viewed the following: