| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible R277AM Polyvinyl Chloride + NBR (PVC+NBR).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.19 g/cc | 1.19 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 51 | 51 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 8.27 MPa | 1200 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 450 % | 450 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -47.8 °C | -54.0 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 182 - 193 °C | 360 - 379 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Low Gloss | |
| Oil Resistant | ||
| Forms | Pellets | |
| Generic Material | PVC+NBR | |
| Generic Name | Polyvinyl Chloride + NBR (PVC+NBR) | |
| Processing Method | Blow Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Footwear |