PolyOne Geon™ Vinyl Flexible R290AE Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible R290AE Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 60 - 64
60 - 64
15 sec; ASTM D2240
Tensile Strength at Break 23.8 MPa
3450 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 200 %
200 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -2.78 °C
27.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 179 - 191 °C
354 - 376 °F
193 - 210 °C
379 - 410 °F
Descriptive Properties Value Comments
Additive UV Stabilizer
Appearance Clear/Transparent
Features High Gloss
UV Absorbing
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Profile Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Profiles