| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible R295AE Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 75 | 75 | 15 sec; ASTM D2240 |
| 82 | 82 | ASTM D2240 | |
| Tensile Strength at Break | 15.3 MPa | 2220 psi | Type IV, 510 mm/min; ASTM D638 |
| Tensile Strength | 8.10 MPa @Strain 100 % |
1170 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 330 % | 330 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -37.2 °C | -35.0 °F | ASTM D746 |
| Flame Spread | 0.00 mm/min | 0.00 in/min | Automotive Burn Test; FMVSS 302 |
| Oxygen Index | 25 % @Thickness 3.18 mm |
25 % @Thickness 0.125 in |
ASTM D2863 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 166 - 177 °C | 331 - 351 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | High Gloss | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Coating Applications |