| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Packaging 2210 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
| Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 81 | 81 | ASTM D2240 |
| Tensile Strength, Yield | 43.8 MPa | 6350 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.35 GPa | 341 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
| Flexural Modulus | 2.61 GPa | 379 ksi | ASTM D790 |
| Izod Impact, Notched | 10.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 61.1 °C @Thickness 3.18 mm |
142 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | FDA Food Contact, Unspecified Rating | |
| Appearance | Clear/Transparent | |
| Features | Food Contact Acceptable | |
| High Gloss | ||
| High Impact Resistance | ||
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Blow Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Bottles | |
| Packaging |