| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Packaging 4195 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
| Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 82 | 82 | ASTM D2240 |
| Tensile Strength, Yield | 52.5 MPa | 7610 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.76 GPa | 400 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
| Flexural Modulus | 2.55 GPa | 370 ksi | ASTM D790 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 83.9 °C <br>@Thickness 3.18 mm |
183 °F <br>@Thickness 0.125 in |
Annealed; ASTM D648 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 78 % <br>@Thickness 0.508 mm,<br> Wavelength 400 nm |
78 % <br>@Thickness 0.0200 in,<br> Wavelength 400 nm |
Internal Method |
| 84 % <br>@Thickness 0.508 mm,<br> Wavelength 700 nm |
84 % <br>@Thickness 0.0200 in,<br> Wavelength 700 nm |
Internal Method |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | FDA Food Contact, Unspecified Rating | |
| Appearance | Clear/Transparent | |
| Features | Food Contact Acceptable | |
| High Gloss | ||
| High Impact Resistance | ||
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Blow Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Bottles | |
| Packaging |